B. Short answer questions
Give reasons:
- a.The wet process of cement manufacture is not used nowadays.
- b.Gypsum is added to clinker during grinding.
- c.OPC is not suitable for mass concrete work.
- d.PPC is preferred for construction in a marine environment.
Answer
- a.The slurry fed to a wet kiln is 30–40% water, all of which must be evaporated in the kiln, so the wet process burns about twice the fuel of the dry process and needs longer kilns. With fuel dear and CO₂ a concern, the dry process with preheaters has replaced it.
- b.To control the setting time. Without gypsum, tricalcium aluminate reacts with water at once and the cement stiffens within minutes (flash setting). Gypsum reacts with it and coats it, giving an hour or more to mix, carry and place the concrete. It is added after the kiln because it would decompose in the heat.
- c.OPC gives out a lot of heat as it hydrates. In a large mass of concrete (a dam, a thick foundation) the heat can’t escape: the inside becomes hot and expands while the outside cools and shrinks, so the mass cracks.
- d.Sea water contains chlorides and sulphates. In PPC the pozzolana uses up the calcium hydroxide (which those salts attack) to form more calcium silicate hydrate, making the concrete denser and less permeable, so salts can’t get in to attack it or to rust the steel bars inside.
Define cement. Write any two uses of cement.
Answer
Cement is a fine gray powder made by heating limestone and clay (with small amounts of other materials) to about 1450 °C and grinding the clinker formed with a little gypsum; mixed with water it sets and hardens, binding other materials together.
Uses: (i) in concrete for buildings, bridges, roads and dams; (ii) in mortar for joining bricks and stones, and in plaster for covering walls. (Also: concrete pipes, poles and blocks, tiles, water tanks.)
What are the raw materials of cement?
Answer
Calcareous materials (rich in lime): limestone, chalk, marl. Argillaceous materials (silica, alumina, iron oxide): clay, shale, slate. Corrective materials: iron ore, bauxite. Gypsum (CaSO₄·2H₂O), 3–5%, added at the grinding stage to regulate setting. Alternative materials: fly ash, blast-furnace slag. Plus coal as fuel.
What is the function of gypsum in the production of cement?
Answer
Gypsum (CaSO₄·2H₂O), 3–5%, is ground in with the clinker to regulate the setting time. It reacts with tricalcium aluminate as soon as water is added and forms a coating on it, which stops it reacting almost at once (flash setting). So the cement stays workable long enough to be mixed and placed, then sets normally.
Differentiate between:
- a.OPC and PPC
- b.the dry process and the wet process of cement production
Answer
a.
| OPC | PPC |
|---|---|
| clinker + gypsum | clinker + gypsum + pozzolana (fly ash, volcanic ash) |
| high early strength, sets faster | lower early strength, sets slower; equal or higher strength later |
| more heat of hydration | less heat of hydration |
| less resistant to sulphates and chlorides | more durable, less permeable |
| dearer; more CO₂ | cheaper; less CO₂, uses waste |
| grades 33, 43, 53 | not sold in grades |
| bridges, high-rise buildings, precast work | dams, foundations, marine works, plaster, masonry |
b.
| Dry process | Wet process |
|---|---|
| raw materials ground dry into raw meal | raw materials ground with water into a slurry (30–40% water) |
| meal preheated in cyclones by kiln gas | slurry fed straight into the kiln |
| less fuel, shorter kiln | more fuel to evaporate water, longer kiln |
| blending needs air mixing and close control | blends easily |
| used today | old, now rare |
What is clinker? Write its use.
Answer
Clinker is the dark gray, hard, rounded lumps (a few millimeters to a few centimeters across) that come out of the rotary kiln, formed when the raw meal is heated to about 1450 °C. It consists mainly of tricalcium silicate (C₃S), dicalcium silicate (C₂S), tricalcium aluminate (C₃A) and tetracalcium aluminoferrite (C₄AF).
Use: clinker is ground with 3–5% gypsum to make Portland cement (and with fly ash or slag too, for blended cements such as PPC). It is also traded: grinding plants buy clinker and grind it into cement.
What are the stages in the production of cement?
Answer
- Crushing and grinding: limestone and clay are crushed and ground to raw meal.
- Blending: the raw meal is mixed and its composition corrected.
- Burning: in the rotary kiln at 1400–1500 °C, limestone is calcined (CaCO₃ → CaO + CO₂) and CaO reacts with SiO₂, Al₂O₃ and Fe₂O₃ to form clinker (C₂S, C₃S, C₃A, C₄AF).
- Final grinding: the cooled clinker is ground with 3–5% gypsum; the cement is stored and packed.
Give a flow sheet diagram for the production of cement.
Answer
Raw materials (limestone, clay) → crushing and grinding → blending (raw mix homogenization) → burning in the rotary kiln (clinker formation) → cooling of clinker → finish grinding (clinker + gypsum) → storage in silos → packaging or bulk transport → finished cement. See Figure 19.2, and Figure 19.3 for the dry process in full.
What are the challenges faced by the cement industry in Nepal?
Answer
Energy shortages and power cuts; outdated equipment (especially in the state plants); high costs of imported coal and clinker; regulatory barriers (environmental and licensing rules); export restrictions, especially India’s certification requirements; poor roads and logistics; oversupply, causing price wars and financial distress; shortage of skilled workers; environmental impact (dust, quarrying, CO₂); and financial instability with limited access to loans.
Write one advantage and one disadvantage of OPC.
Answer
Advantage: high early strength and fast setting, so formwork can be removed and work can go on sooner (good for precast work, bridges, high-rise buildings).
Disadvantage: high heat of hydration, so it can crack large masses of concrete; it is also less resistant to sulphate and chloride attack, and more costly and polluting (more clinker) than PPC.
What are the merits and demerits of PPC?
Answer
Merits: less heat of hydration (good for mass concrete); better long-term strength and durability; resists sulphates, chlorides and water (marine and hydraulic works); less permeable; better workability and a smoother finish; cheaper; more eco-friendly (uses fly ash, less clinker and CO₂).
Demerits: lower early strength and slower setting, so it needs longer curing and formwork must stay longer; not suited to work needing quick strength (precast, prestressed concrete, urgent repairs); its quality depends on the quality of the fly ash.
What is the function of pozzolanic material in PPC?
Answer
A pozzolana (fly ash, volcanic ash) contains reactive silica that does not set with water by itself, but reacts with the calcium hydroxide released as cement hydrates, forming more calcium silicate hydrate (C–S–H), the main binder. So it turns weak, soluble calcium hydroxide into strong binder: the concrete becomes denser, stronger over time, less permeable and more resistant to chemical attack. It also replaces part of the clinker, lowering the heat of hydration, the cost and the CO₂ emitted.
C. Long answer questions
Describe the stages in the production of cement. Draw a flow sheet diagram showing the different stages of cement production.
Hint
Four stages; for burning, write the calcination equation and the four clinker compounds with their equations.
Answer
- Crushing and grinding. Limestone, clay and correctives (iron ore, bauxite) are quarried, crushed, and ground to a fine powder, the raw meal, stored in silos.
- Blending. The raw meal is blended with compressed air or mechanical mixers and analyzed; the proportions of CaO, SiO₂, Al₂O₃ and Fe₂O₃ are corrected.
- Burning. In the rotary kiln, at 1400–1500 °C: moisture evaporates; limestone is calcined, ; then lime combines with the clay’s oxides: (C₂S), (C₃A), (C₃S), (C₄AF). These form as hard lumps, clinker.
- Final grinding. The clinker is cooled, then ground with 3–5% gypsum (which controls the setting time) to a fine powder, cement, which is stored in silos and packed.
Flow sheet: raw materials → crushing and grinding → blending → burning in rotary kiln (clinker) → cooling → finish grinding with gypsum → storage → packing → cement (Figure 19.2).
Explain the flow sheet diagram for the manufacture of Portland cement by the dry process.
Answer
- Crushing: limestone, clay and other materials are crushed.
- Drying and grinding: they are dried by hot kiln gas and ground in a ball or roller mill to raw meal.
- Blending: the raw meal is tested and homogenized in blending silos.
- Preheating: it falls through a preheater tower of cyclones against the hot exhaust gas of the kiln (and a precalciner completes most of the calcination).
- Clinker formation: in the rotary kiln at about 1450 °C, CaO combines with SiO₂, Al₂O₃ and Fe₂O₃ to give clinker (C₃S, C₂S, C₃A, C₄AF).
- Cooling: the clinker is cooled fast by air in the cooler; the heated air goes to the kiln.
- Grinding with gypsum: clinker + 3–5% gypsum is ground to cement.
- Storage and packaging: in silos, then bags.
Flow sheet: raw materials → crushing and dry grinding → raw meal homogenization → preheater → rotary kiln → clinker formation → clinker cooling → clinker + gypsum → cement grinding → storage, packing and distribution (Figure 19.3).
Describe the whole process of manufacturing Portland cement by the wet process.
Answer
- Crushing: limestone, clay and other materials are crushed.
- Slurry formation: they are mixed with water in a wash mill into a slurry with 30–40% water.
- Grinding: the slurry is ground finer in a ball or tube mill.
- Homogenization: the slurry is stored in tanks and stirred continuously so its composition is uniform; it is analyzed and corrected.
- Clinker formation: the slurry is fed into the upper end of a long rotary kiln. In its first part the water is boiled off; further down, the limestone is calcined; near the flame, at about 1450 °C, the clinker compounds form.
- Cooling: the hot clinker is cooled quickly.
- Grinding with gypsum: clinker + 3–5% gypsum is ground to cement.
- Storage and packaging: the cement is stored in silos and packed.
Flow sheet: raw material crushing → mixing with water (slurry) → grinding of slurry (ball/tube mill) → homogenization (slurry tank) → clinker formation in the rotary kiln → clinker cooling → grinding with gypsum → storage and packaging (Figure 19.4). It blends well but uses much more fuel than the dry process, which is why it is now rarely used.
Differentiate between OPC and PPC.
Answer
| Feature | OPC | PPC |
|---|---|---|
| Raw materials | clinker (limestone + clay) and gypsum | clinker, gypsum and pozzolana (fly ash, volcanic ash) |
| Composition | mainly clinker | less clinker, plus pozzolana |
| Early strength | high | lower |
| Long-term strength | good | equal or higher |
| Setting | faster | slower |
| Heat of hydration | more; can crack mass concrete | less; good for mass concrete |
| Durability | less resistant to sulphates and chlorides | more resistant; less permeable |
| Workability | needs more water | better |
| Cost | dearer | cheaper |
| Environment | more energy and CO₂ | less energy and CO₂; recycles waste |
| Grades | 33, 43, 53 | not graded |
| Uses | high-rise buildings, bridges, precast and prestressed work | dams, foundations, marine and hydraulic works, plaster, masonry |
Write a note on the cement industry in Nepal.
Answer
Cement is one of Nepal’s biggest industries. The public sector started it: Himal Cement at Chobhar (Nepal’s first, closed in 2002 over its dust in the Kathmandu Valley), Hetauda Cement in Makwanpur (opened in 1986, 750 tonnes a day) and Udayapur Cement at Jaljale (built with Japanese help, production from 1992–93, 800 tonnes a day). The two remaining state plants, with old machinery and large debts, run far below capacity or not at all.
The private sector now makes almost all of Nepal’s cement: about 65 plants in 2023 (23 that make clinker, 42 that only grind it), such as Hongshi-Shivam, Arghakhanchi, Sagarmatha, Maruti, Jagdamba, Ambe, Pashupati and many more; in 2024 the plants could make about 22 million tonnes a year, with Rs 300 billion invested and about 15,000 people employed. Nepal, which once had to import cement, is now nearly self-sufficient, using about 8 million tonnes a year (2024), and exports cement and clinker (Rs 3.85 billion in 2023/24), helped by an export incentive and power tariff discounts.
Challenges: power shortages, outdated equipment, dear imported coal and clinker, rules and licensing, trade barriers (India’s certification), poor roads, oversupply and price wars, few skilled workers, pollution and CO₂, and limited finance. The industry gives jobs, saves foreign currency and supplies the country’s roads, hydropower projects and buildings.